I am not an expert, please enlighten me!
6061 is highly weldable, for example using tungsten inert gas welding (TIG) or metal inert gas welding (MIG). Typically, after welding, the properties near the weld are those of 6061-O, a loss of strength of around 80%. The material can be re-heat-treated to restore -T4 or -T6 temper for the whole piece. After welding, the material can naturally age and restore some of its strength as well. Nevertheless, the Alcoa Structural Handbook recommends the design strength of the material adjacent to the weld to be taken as 76 MPa (11,000 psi) without proper heat treatment after the weld.[citation needed] Typical filler material is 4043 or 5356.